Effect of ZnO electrical conductivity on the composition of hexagonal and cubic phases in MgxZn1-xO ceramics

Fr4.5
6 Nov 2026, 15:01
4m
Online (Zoom)

Online (Zoom)

Poster Optics and High Technology Material Science Rapid Poster Sessions

Speaker

Oleksandr Melnichuk (Nizhyn Mykola Gogol State University, Nizhyn, Ukraine)

Description

The influence of the electrical conductivity of the initial ZnO powder on the structural, optical properties and chemical composition of MgxZn1-xO ceramics was investigated. Ceramic samples containing 10-30 mol.% Mg were prepared from ZnO and MgO powders and sintered in air at 1050 °C for 3 h. Two series of samples were prepared using ZnO powders with different electrical conductivities. Photoluminescence (PL), photoluminescence excitation (PLE) spectroscopy, scanning electron microscopy (SEM), and energy-dispersive X-ray spectroscopy (EDX) were used to investigate the formation and composition of the solid-solution phases.

The optical spectra revealed a more pronounced blue shift of the excitonic peak in samples prepared from low-resistive ZnO powder, indicating a higher Mg content in the hexagonal phase. EDX analysis confirmed that increasing the electrical conductivity of the initial ZnO powder resulted in higher Mg content in the hexagonal-phase grains and higher Zn content in the cubic-phase grains. In Mg0.2Zn0.8O ceramics prepared from high-resistive ZnO powder, the Mg content in the hexagonal phase was approximately 5-6 %, whereas the Zn content in the cubic phase was 10-11 %. In samples prepared from low-resistive powder, these values increased to 9-12 % Mg and approximately 17 % Zn, respectively. The results indicate that the formation and chemical composition of both phases depend on the electrical conductivity of the initial ZnO powder that is determined by concentration of interstitial zinc. A possible mechanism is proposed in which interstitial Zn migrates to grain boundaries and incorporates into MgO, promoting Mg enrichment of the grain boundaries due to self-compensation process. This facilitates the incorporation of Mg into ZnO and may promote the simultaneous formation of the hexagonal and cubic solid-solution phases during sintering. The findings demonstrate that the defect structure of the starting powder is an important factor governing the phase composition of MgxZn1-xO ceramics.

Keywords: MgxZn1-xO ceramics, ZnO electrical conductivity, interstitial zinc, hexagonal phase, cubic phase, photoluminescence, EDX.

Author

Oleksandr Melnichuk (Nizhyn Mykola Gogol State University, Nizhyn, Ukraine)

Co-authors

Nadiia Korsunska (V. Lashkaryov Institute of Semiconductor Physics of the National Academy of Sciences of Ukraine, Kyiv, Ukraine) Liudmyla Melnichuk (Nizhyn Mykola Gogol State University, Nizhyn, Ukraine) Maksym Strilets (Nizhyn Mykola Gogol State University, Nizhyn, Ukraine) Larysa Khomenkova (V. Lashkaryov Institute of Semiconductor Physics of the National Academy of Sciences of Ukraine, Kyiv, Ukraine)

Presentation materials

There are no materials yet.